Two major reasons why the one-component silicone PU does not dry or dry slowly on the construction site

  The curing principle of one-component silicone PU is moisture curing (or called water vapor curing), so the glue forming medium on site is water vapor. During the construction process, the material does not dry or dry slowly, and the reason is only insufficient water and dilution. There are two main reasons for the mismatch of agents. FOSHAN GRK COMMERCIAL CO LTD is one of the Chinese supplier for the silicone PU ,with good price and best service. whatsApp:008613660776067 ,facebook: paintfloor.GRK 1. Not dry or slow dry due to insufficient water When the air humidity is appropriate and the basic dryness is appropriate, the amount of water required for each company's product formulation design is not necessarily the same. In order to make it easy for the construction team to adjust on site and avoid accidents when doing things based on the feeling, Greens berg  improved the production process during the production of the factory, vacuumed the materials, and carried out the second